Skip to main content
. 2016 Sep 9;12:6–12. doi: 10.1016/j.btre.2016.09.001

Fig. 3.

Fig. 3

Size and distribution of pores in protein hydrogels treated with a salt-leaching procedure. (A) Size distribution of pores within the protein hydrogels matrix. The used NaCl crystals were grinded with a pestle and mortar for a specific times: (B) 10 min. (C) 2 min. (D) 1 min. (E) not grinded. Protein hydrogels were stained with rhodamine B and investigated via confocal laser scanning microscopy. Scale bar 50 μm.