Figure 2.

Figure 2

(a) High-resolution TEM image showing the morphology of a SLG deposited with 180 cycles of TiO2 at 60 °C and (b) the corresponding SAED pattern. (c) Formation of the crystalline grains in the sample after in situ annealing at 400 °C and (d) the corresponding SAED pattern. (e) Color-coded BF image showing the distribution of the grains after annealing.