Skip to main content
. 2017 Mar 21;12:2205–2213. doi: 10.2147/IJN.S123417

Figure 3.

Figure 3

SEM image of fabricated electrospun mat.

Note: SEM image at 1,000× of electrospun nanofibers of PEO 8% (wt/v) using the following electrospinning conditions of 10 cm, 18 kV, and 0.3 mL/h.

Abbreviations: SEM, scanning electron microscopy; PEO, polyethylene oxide; v, volume; wt, weight; HV, high voltage; Mag, magnification; WD, working distance.