XRD images of (a) bare-Pd/Fe, (b) HPMC-Pd/Fe, and (c) PAC- Pd/Fe NPs. Fe loading is 0.4 g L-1 with Pd 0.3 wt% of Fe, cellulose is 1 g L-1.