Skip to main content
. 2017 Mar 31;12:241. doi: 10.1186/s11671-017-2001-4

Fig. 2.

Fig. 2

a Comparison of transparent strips made from initial OSP. b OSP after ultrasound treatment. CNF films prepared after hydrolysis by sulfuric acid of concentration 43% at (c) 20 °C, 30 min; d 20 °C, 60 min; e 60 °C, 30 min; f and 60 °C, 60 min. The duration of ultrasound treatment all patterns was 30 min