Skip to main content
. 2017 Mar 31;12:241. doi: 10.1186/s11671-017-2001-4

Fig. 5.

Fig. 5

TEM images of nanocellulose prepared by hydrolysis with H2SO4 concentration 43% at 40 °C and ultrasound treatment for 30 min