Skip to main content
. 2017 Mar 31;7:45776. doi: 10.1038/srep45776

Figure 2.

Figure 2

(a) Typical microscope images of the microbubbles created on the gold nanoisland films in water with (W) and without (W/O) degassing during (t = 0–5 s) and after (t = 5–10 s) laser heating. (b) The detailed time dependence of the bubble diameter, where the capital letters correspond to those in (a). The results of three measurements are displayed for both water W and W/O degassing.