Table 1.

Effects of different concentrations of EL and ES on the diameter of blank NFs

Polymer concentration (%) EL-NF diameter (nm) ± SD ES-NF diameter (nm) ± SD
10 51.2d±22.7 69.7d±24.8
15 124.4c±50.3 171.4c±37.2
20 295.2b±91.2 590.4b±156.2
25 355.7a±117.2 864.4a±371.8

Notes: The feeding rate was 0.5 mL/h at an applied voltage of 15 kV. a > b > c > d.

Abbreviations: EL, Eudragit L100; ES, Eudragit S100; NF, nanofiber; SD, standard deviation.