Skip to main content
. 2016 Nov 4;9(1):24–32. doi: 10.1038/ijos.2016.40

Table 1. ARI scores of orthodontic cements.

    ARI scores (n=10)*
 
Group Solution aging 0 1 2 3 SIG
PEHB+NACP 1 day 2 3 5 0 A
TB control 1 day 1 2 6 1 A
VT control 1 day 3 6 1 0 B
PEHB+NACP 70 days 1 3 6 0 A
TB control 70 days 1 3 6 0 A
VT control 70 days 4 5 1 0 B

ARI, adhesive remnant index; NACP, nanoparticles of amorphous calcium phosphate; SIG, statistical significance; TB, Transbond XT; VT, Vitremer.

ARI: 0=no adhesive left on the tooth surface; 1=less than half of the adhesive was left on the tooth surface; 2=half or more of the adhesive was left on the tooth; 3=the entire adhesive was left on the tooth surface.

Different letters (A, B) indicating significant differences in the ARI scores (P<0.05).