Skip to main content
. 2017 Mar 1;54(5):1168–1174. doi: 10.1007/s13197-017-2553-4

Table 3.

Power-law parameters for the elastic modulus for WPI gels (8%, w/v) including different concentrations of kefiran as determined by frequency sweep test

Parameters Kefiran concentration (%, w/v)
0 0.02 0.04 0.08
a (Pa.s) 9.759 ± 0.29a 12.463 ± 1.11b 14.544 ± 1.21b 24.047 ± 1.10c
b 0.090 ± 0.003a 0.108 ± 0.003b 0.115 ± 0.004b 0.126 ± 0.002c

Values represent the mean ± standard deviation of three independent experiments

Means within the same row with different superscript letters are significantly different (P < 0.05)