Skip to main content
. 2014 Nov 5;4:6913. doi: 10.1038/srep06913

Figure 5. IEAP material D: A non-ionic polymer (PVdF-HFP) membrane with CDC electrodes and electrolyte EMIBF427.

Figure 5

Checkpoint F is marked at 5000 working cycles. Exposure to UV radiation significantly damages this IEAP material, although it is able to function with lower performance. Vacuuming increases the degradation during operation.