Figure 3. The properties of 30 supercapacitor samples with NaCl electrolyte.

Figure 3

(a) ESR plotted against the average sheet resistance of the two current collectors in the device; (b) the specific capacitance plotted against activated carbon ink mass of both electrodes; (c) the leakage current measured after 1 h hold at 0.9 V plotted against device capacitance.