Table 2. The means (standard deviations) of marginal gaps in µm .
Composite resin type | Composite resin temperature | Intra-group P-value | |
Room temperature | After 40 cycles of preheating | ||
Dimethacrylate | 35.9 (4.7) | 20.2 (3.2) | <0.001* |
Silorane | 22.2 (3.3) | 14.4 (2.2) | <0.001* |
Inter-groupP-value | <0.001* | <0.001* | — |
* Statistically significant