Skip to main content
. 2017 Apr 12;2017:1797091. doi: 10.1155/2017/1797091

Table 2.

Mean hardness number and crosslink density of the tested bulk fill composite resins after dry storage, storage in 75% ethanol, and storage in 100% methyl ethyl ketone.

Bulk fill composite resin Dry storage Storage in 75% E Storage in 100% MEK P  value
SureFill
 Vickers hardness number (SD) 82.4 (2.4) 76.6 (2.1) 74.6 (1.7)
 Crosslink density (SD) 7.0 (1.4) 9.4 (2.5) 0.02

SonicFill
 Vickers hardness number (SD) 99.0 (1.3) 88.5 (1.6) 87.2 (1.8)
 Crosslink density (SD) 10.5 (1.8) 11.9 (1.3) 0.06

P  value <0.0001 0.02

SD: standard deviation.

P value of t-test comparing differences after using solvents in each material.

P value of t-test comparing the two materials when each solvent was used.

Statistically significant difference at P ≤ 0.05.