Figure 5.

Figure 5

SEM images of filaments from 0.8 mm diameter (a) as-drawn wire, and wire after 100 atm OP at 820 °C for (b) 2 h and (c) 12 h. The cracks visible in the as-drawn filaments in (a) occurred during etching.