Skip to main content
. Author manuscript; available in PMC: 2017 Oct 1.
Published in final edited form as: Supercond Sci Technol. 2016 Aug 19;29(10):105005. doi: 10.1088/0953-2048/29/10/105005

Figure 7.

Figure 7

(a) Diameter, and (b) JC and n-value at 4.2 K and 5 T of a 2.2 m long wire after full heat treatment at 100 atm with both ends fully open. The diameter of the as-drawn wire and the diameter of the fully densified short wire that had both ends closed are shown for reference. JC is calculated as the ratio of IC to the densified cross section area of the filaments (2212 + voids) measured after 820 °C for 12 h at 50 atm.