Published in final edited form as: Supercond Sci Technol. 2016 Aug 19;29(10):105005. doi: 10.1088/0953-2048/29/10/105005

Figure 8.

Figure 8

JC at 4.2 K and 5 T (from Fig. 7b) as a function of the decrease in wire diameter after full heat treatment at 100 atm with both ends fully open for a 2.2 m long wire. The dashed line is a guide for the eyes.