Skip to main content
. 2017 Mar 24;17(4):673. doi: 10.3390/s17040673

Figure 12.

Figure 12

Images for sewn the nickel-plated copper wire without TPU: (a) Before wash test; (b) 5 cycles of wash test; (c) 20 cycles of wash test; (d) 30 cycles of wash test with TPU; (e) Before wash test; (f) 5 cycles of wash test; (g) 20 cycles of wash test; (h) 50 cycles of wash test.