Table 1.
Correlation of elemental ratios measured in this study, with X-ray diffraction measurements made on the same 39 calcifications in a previous study.
EDS Measurement | XRD measurement | Coefficient | Adjusted R2 | p-value | Adjusted p-value |
---|---|---|---|---|---|
Mg:Ca Ratio | Whitlockite % | −35.6 | 0.183 | 0.004 | 0.034 |
Domain Diameter | −125 | 0.165 | 0.007 | 0.046 | |
‘c’/‘a’ lattice parameter ratio | −0.105 | 0.279 | <0.001 | 0.003 | |
Ca:P Ratio | Whitlockite % | 2.73 | 0.098 | 0.032 | 0.158 |
Domain Diameter | −0.0555 | −0.028 | 0.991 | 1.000 | |
‘c’/‘a’ lattice parameter ratio | 0.00231 | −0.012 | 0.459 | 1.000 | |
Na:Ca Ratio | Whitlockite % | −1.29 | −0.027 | 0.871 | 1.000 |
Domain Diameter | 63.1 | 0.107 | 0.026 | 0.154 | |
‘c’/‘a’ lattice parameter ratio | 0.0366 | 0.071 | 0.056 | 0.222 |