Table 3.

Table showing change in contact angle of the LDPE film

Sample Contact angle
Control 98.6 ± 3.5
After 10 days 70 °C thermal treatment 91.5 ± 3.5
After 30 days incubation with Rhizopus 67 ± 2.6

The result represents the average of three independent experiments