Skip to main content
. 2017 Apr 26;7:1173. doi: 10.1038/s41598-017-01214-4

Figure 7.

Figure 7

SEM images and EDX analysis of corrosion products surrounding expanded helical stents under the flow induced wall shear stress value of 0.154 Pa for 3 days in DMEM (10% FBS, 1% P/S) at 37 °C, 5% CO2. aIndicates Mg-based helical stent has been implanted.