(a) Hardness as a function of the penetration depth obtained by CSM method for RGO/Cu composites which containing 0–7 mg/L GO in the electrolyte. The fitting curve was superimposed on this graph and five indentation data for each sample were used in statistical calculations. (b) Curve of ultimate hardness of RGO/Cu composites.