Skip to main content
. 2017 May 3;7:1483. doi: 10.1038/s41598-017-01488-8

Figure 3.

Figure 3

The D2 permeance and the kinetic selectivity under different strains for temperature ranging from 20 to 200 K. Different colors indicate different strains ranging from 0% to 6%. The dashed lines indicate the industrial-acceptable values for permeance (6.7 × 10−8 mol/s/cm2/bar) and selectivity (6), respectively.