Table 2.
Textural properties of MoO3 prepared on different temperature.
| Sintering Temperature (°C) | BET surface area (m 2 /g) | Pore volume (cm 3 /g) | Pore size (nm) |
|---|---|---|---|
| 300 | 22.20 | 0.09 | 15.86 |
| 400 | 25.62 | 0.13 | 20.76 |
| 500 | 8.95 | 0.04 | 19.60 |
| 600 | 10.63 | 0.07 | 21.90 |
Textural properties of MoO3 prepared on different temperature.
| Sintering Temperature (°C) | BET surface area (m 2 /g) | Pore volume (cm 3 /g) | Pore size (nm) |
|---|---|---|---|
| 300 | 22.20 | 0.09 | 15.86 |
| 400 | 25.62 | 0.13 | 20.76 |
| 500 | 8.95 | 0.04 | 19.60 |
| 600 | 10.63 | 0.07 | 21.90 |