Skip to main content
. 2017 Feb 2;6:39–48. doi: 10.1007/s40204-017-0062-1

Table 3.

Optimized electrospinning parameters for mats with different curcumin loadings

Mat composition Parameters
Feeding rate (mL h−1) Working distance (mm) V (kV) Polymer. conc. (wt%)
PCL 1 160 18.4 12.5
PCL/1% CU 1 160 18 12.5
PCL/8.5% CU 1 160 17.8 12.5
PCL/16% CU 1 160 17.8 12.5