. 2017 May 19;21:7. doi: 10.1186/s40824-017-0093-7

Fig. 2.

Fig. 2

SEM micrographs of a fracture surface of a 20%PEEK/80%CS specimen prepared at a P:L ratio of 0.85 g/mL (a) prior to heat treatment and (b) after heat treatment. (c) FT-IR spectra between 500 cm−1 and 4000 cm−1 wavenumbers of PEEK and CSH (CaSO4.0.5H2O) starting powders, and a powdered 20%PEEK/80%CS specimen after heat treatment