Figure 4.

Figure 4

(A) Porosity, (B) changes of water absorption, (C) weight loss of (a) NMPC and (b) MPC scaffolds, (D) changes of pH of solution after (a) NMPC and (b) MPC scaffolds soaking in PBS with time.

Abbreviations: NMS, nanoporous magnesium silicate; PBSu, poly(butylene succinate); NMPC, NMS/PBSu composite; MS, magnesium silicate; MPC, MS/PBSu composite; PBS, phosphate-buffered saline.