Skip to main content
. 2017 May 23;7:2282. doi: 10.1038/s41598-017-02511-8

Figure 3.

Figure 3

FE-SEM images of (AC) AgNW-based micropatterns on a glass substrate before the pattern transfer process and (DF) AgNW-based micropatterns on a hydrogel substrate after pattern transfer process. The line pattern width is 200 μm.