Mechanical flexibility or stability of AgNW-based micropatterns was measured by digital multi-tester device and compared to the initial value. (A) Bending test of AgNW-based micropatterns (700 μm in width and 2 cm in length) on PEG hydrogel. (B) Stability test of AgNW-based micropatterns on PEG hydrogel in DI water. (C) The I–V performance of the AgNW-micropatterns (500 μm in width, 2 cm in length) on hydrogel before bending and in bending state. The inset shows the LED emission with flexible AgNW-based micropatterns (500 μm in width and 2 cm in length) on agarose hydrogel.