(a) LSVs measured at NiSe2 (Electrodeposited) @ Au, NiSe2 (Hydrothermal) @ CFP, RuO2 @ Au and bare Au at in N2 saturated 1.0 M KOH solution at a scan rate of 10 mV s−1. (b) CVs measured under identical condition to estimate the overpotential at 10 mA cm−2. (c) Tafel plots of catalysts.