Skip to main content
. 2009 Aug 28;2(3):1104–1126. doi: 10.3390/ma2031104

Figure 11.

Figure 11

Relation between the rate of enzymatic erosion and the degree of crystallinity (Xc) (A) and the lamellar thickness (B) for melt-crystallized PHA films and solvent-cast, stretched, and stretched-annealed UHMW-P(3HB) films. [41,74] Reproduced with permission from Abe et al., Macromolecules; published by ACS, 1998.