Skip to main content
. 2010 Jul 13;3(7):4051–4065. doi: 10.3390/ma3074051

Table 1.

Properties of the synthesized MnFe2O4 nanoparticles. Values for SAR are reported for a 7 mg/mL or 0.349 wt % aqueous nanoparticle solution. Reported errors represent the standard deviations for three replicates.

Sample EDC
Linker
Concen-
tration
TEM Particle
Diameter
(nm)
DLS Particle
Diameter
(nm)
Magnetization
at 10 kOe
(emu/g)
SAR (W/g) at 653 Oe, 266 kHz
DMSA-
MnFe2O4
- 12.1 ± 0.4 34 ± 1.2 44.1 1.45
Chitosan-
MnFe2O4
0.3 wt % 17.2 ± 1.3 94.4 ± 2.6 40.2 1.20
0.6 wt % 17.7 ± 2.1 98.2 ± 3.2 39.8 1.17
0.9 wt % 18.3 ± 1.6 104.2 ± 2.4 31.2 1.08
1.2 wt % 17.1 ± 1.3 96.8 ± 2.2 36.7 1.15