Figure 3.

Figure 3

Comparison of bone-like apatite formation on plasma sprayed CaO-SiO2 based bioceramic coatings after immersion in SBF solution: (a) CaSiO3 coating immersed in SBF solution for 1 day. (b). Ca2SiO4 coating immersed in SBF solution for 1 day. (c) CaMgSi2O6 coating immersed in SBF solution for 5 days. (Figure 3a and b are reprinted with the permission from Liu, X.Y. [204,205]; Figure 3c is reprinted with the permission from Xue, W.C. [207])