. 2010 Jul 9;3(7):3994–4050. doi: 10.3390/ma3073994

Figure 4.

Figure 4

Comparison of bone-like apatite formation on plasma sprayed zirconia coatings after immersed in SBF solution for 28 days. (a) undoped zirconia coating. (b) zirconia coating stabilized 12.8 mol % calcia. (c) zirconia coating stabilized with 16 mol % calcia. (d) zirconia coating stabilized with 30 mol % calcia.