Skip to main content
. 2011 May 17;4(5):908–928. doi: 10.3390/ma4050908

Figure 7.

Figure 7

Temperature dependent magnetization measurements performed on samples with equal porous silicon morphology (pore-diameter ~90 nm, distance between the pores ~35 nm) infiltrated with two different concentrations of the iron oxide particle solution (triangles, initial concentration; squares, half of initial concentration). The average particle-size is 8 nm [37].