Skip to main content
. 2011 Aug 10;4(8):1384–1398. doi: 10.3390/ma4081384

Figure 5.

Figure 5

Molecular weight distribution curves of PLA (a), PBA (b), PHA (c), and PDA (d) before hydrolytic degradation (0 days) and after hydrolytic degradation at 80 °C for 4 days.