Skip to main content
. 2011 Aug 10;4(8):1384–1398. doi: 10.3390/ma4081384

Figure 7.

Figure 7

Weight loss of PLA, PBA, PHA, and PDA during hydrolytic degradation at 37 °C, as a function of degradation time.