. 2013 Feb 22;6(2):682–698. doi: 10.3390/ma6020682

Figure 2.

Figure 2

Scanning electron microscope (SEM) micrographs of the fractured surface of the agarose/talc composite films with (a) 0 wt %; (b) 2 wt %; (c) 4 wt %; (d) 6 wt %; (e) 8 wt % and (f) 10 wt % of BmimCl/Urea at magnification of 1000×.