Table 1.

Concentration (in at. %) of carbon (C), oxygen (O), nitrogen (N) and sulfur (S), determined by XPS analysis, on HDPE and LDPE treated with plasma for 50 s (50), and subsequently grafted with fibronectin (Fn) and bovine serum albumin (BSA). Mean from three measurements for each experimental group; the measurement error did not exceed 5%.

Material/Modification HDPE LDPE
C (at. %) O (at. %) N (at. %) S (at. %) C (at. %) O (at. %) N (at. %) S (at. %)
50 82.2 14.2 2.5 0 83.0 14.8 1.5 0
50 Fn 72.9 20.2 6.7 0.2 82.2 13.6 2.8 at limit of detection
50 BSA 74.4 15.3 9.9 0.4 72.7 15.3 10.9 0.4