Figure 9.
The densification behavior of Fe nanopowders with optimal agglomerate size during heat-up with a heating rate of 10 °C/min and subsequent isothermal sintering at 700 °C in a hydrogen atmosphere [12].
The densification behavior of Fe nanopowders with optimal agglomerate size during heat-up with a heating rate of 10 °C/min and subsequent isothermal sintering at 700 °C in a hydrogen atmosphere [12].