Skip to main content
. 2013 Oct 22;6(10):4776–4786. doi: 10.3390/ma6104776

Figure 2.

Figure 2

Resistivity and longitudinal strain data versus time for different samples of a BFS composite with 0.76% CF (by BFS mass). Loading rate was 200 N/s in all tests, and the maximum compressive stress was change between tests.