. 2014 Feb 10;7(2):1017–1045. doi: 10.3390/ma7021017

Figure 12.

Figure 12.

TEM images of cellulose acetate nanofibers containing 5 wt% AgNO3 (A) before UV irradiation and (B) after UV irradiation [70].