Skip to main content
. 2014 May 6;7(5):3588–3622. doi: 10.3390/ma7053588

Figure 12.

Figure 12.

X-ray diffraction (XRD) peaks: (A) for porous green body after Mg removal; (B) for Ti/Mg compact; (C) for compact packed only with Ti powder; (D) energy-dispersive X-ray spectroscopy (EDS) peaks for porous green body after Mg removal (initial Mg content of 60 vol%). Reprinted with permission from [72]. Copyright 2013, Elsevier.