Skip to main content
. 2014 May 21;7(5):4001–4018. doi: 10.3390/ma7054001

Figure 10.

Figure 10.

SEM micrographs of a TCP/PLA specimen after bending test: (a) fracture surface at low magnification; and (b) detail of fracture surface within a rod. Short microfibrils but no macrofibrils are evident.