. 2015 Feb 16;8(2):751–783. doi: 10.3390/ma8020751

Figure 23.

Figure 23

(a) Flank wear; and (b) crater wear progressions in turning test for AISI 316L steel with different non-metallic inclusions: (1)—alumina (Al2O3); (2)—gehlenite (2CaO·Al2O3·SiO2); and (3)—anorthite (CaO·Al2O3·2SiO2) [42].