Skip to main content
. 2015 Mar 4;8(3):914–931. doi: 10.3390/ma8030914

Figure 5.

Figure 5

Figure 5

(a) The XRD patterns and (b) microstructure of alloys form Fe-Al system for various Al content 65.5 at%, 68 at%, 70 at%, 72 at% and 77.5 at%, as casted and annealed at temperature of 1050 °C for 100 h.