Skip to main content
. 2015 Mar 2;8(3):850–866. doi: 10.3390/ma8030850

Table 3.

Resin shear bond strength of the zirconia ceramic specimens subjected to different surface treatments before and after thermocycling (mean (standard deviation) in MPa).

Group 24 h-Water Storage 5000 Thermocycling
APA 6.6 (1.1) Aa 3.7 (0.6) Ab
10F5 8.3 (1.2) Aa 4.9 (0.8) Bb
10F30 13.5 (1.6) Ba 11.5 (1.8) CDb
20F5 12.6 (2.8) Ba 9.6 (2.1) Cb
20F30 25.2 (3.0) Ca 21.0 (3.0) Eb
30F5 14.9 (2.7) Ba 12.7 (1.6) Db
30F30 34.7 (4.1) Da 29.8 (3.9) Fb

Within the same column, means with the same uppercase letter are not statistically different (p > 0.05). Within the same row, means with the same lowercase letter are not statistically different (p > 0.05).