Properties of hemp, silk, and soy silk fiber, and poly(vinyl alcohol) (PVOH)/clay aerogel. The shear modulus and shear strength were taken to be equal to those of expanded polystyrene with the same density.

Property Hemp Fiber Silk Fiber Soy Silk Fiber PVOH/Clay Aerogel
Strain Elongation (%) 1.6 14 18 -
Tensile Strength (MPa) 690 120 5 -
Elastic Modulus (GPa) 12.1 7 2.6 0.015
Density (g/cm3) - 1.34 1.29 0.05
Shear modulus (MPa) - - - 1.93
Shear Strength (kPa) - - - 124