Figure 2.

Figure 2

Light microscope (AD; scale bar: 700 µm) and scanning electron microscope pictures (EH; scale bar: 900 µm) of the Ti-6Al-4V scaffolds with four basic structures and fabricated with two different processes (EBM: electron beam melting; SLM: selective laser melting).