Figure 28.
Force vs. time slow strain rate test (SSRT) curves for SAF 2507 in 30 wt% MgCl2 solution at 180 °C at a strain rate of 3.7 × 10−7/s with different NO2− concentrations, reprinted with permission from [72]. Copyright 2010 Elsevier.
Force vs. time slow strain rate test (SSRT) curves for SAF 2507 in 30 wt% MgCl2 solution at 180 °C at a strain rate of 3.7 × 10−7/s with different NO2− concentrations, reprinted with permission from [72]. Copyright 2010 Elsevier.